Cookie Img
Send Inquiry Send SMS
Visaka Designer Boards  Banner
Home » Products » VBoards » Mezzanine Floor

Mezzanine Floor

Mezzanine Floor
Mezzanine Floor
Product Code : 15
Product Description

Mezzanine Floor

Backed with expertise and knowledge in this domain, we are counted amongst the foremost manufacturers and exporters of Mezzanine Floor. This type of floor is broadly acknowledged among our long list of esteemed clients. Our offered Mezzanine Floor is wisely manufactured at our state of the art production unit. We make sure that our entire assortment of raw materials for manufacturing these floors is sourced from only reliable vendors. A wide range of floors is offered to our clients at competitive prices.

Available in thickness of 18, 20, 25mm

COMPOSITION:
V-Board range of fibre cement boards is manufactured from a homogenous mixture of Portland Cement, treated cellulose fibres, finely ground silica and quartz and other select mineralfillers in a state-of-the-art unit using sophisticated, digitally -controlled processes. The principle components of the mixture are cement and cellulose fibre. Cement acts as a hydraulic binder and the cellulose fibres interlock with the cement and quartz matrices to add strength to the boards. No asbestos is used during the entire process, making V-Board products 100% asbestos free.



Application

Thickness (mm)

Internal

4

6

8

10

12

14

16

18

20

25

False Ceiling

Yes

Yes









Partitions



Yes

Yes

Yes






Wall cladding




Yes

Yes






Mezzanine Flooring








Yes

Yes

Yes

Doors





Yes

Yes

Yes




External











Prefab Structure



Yes

Yes







Wall Cladding



Yes

Yes







Sign Boards


Yes

Yes








Technical Specification

(V-Board manufactured as per IS- 14862:2000, Type B Category '3')



Properties

Units

Performance

Apparent Density

Kg/m3

>1250

Standard Weight (For 6mm)

Kg/m2

7.5

Mechanical Characteristics



Minimum Moulds of rupture at EMC

Mpa,N/mm2

>10.5

Rupture(MOR) IN WET Condition

Mpa,N/mm2

>6.0

Impact Strength (Charpy Method)

KJ/m2

4.3 wet, 1.7 Dry

Adhesion/Lamina Bond Strength

Map, N/mm2

0.9 to 1.0

Additional Characteristics



Thermal Conductivity at (50oC Mean Temperature)

W/m .k

0.21

Linear Coefficient of thermal expansion

Per deg c

7.5 x 10 E-6

pH value

(72 hours)

12

Acoustic insulation

dB

26 (6mm V-Board)35 with 50mm Mineral wool 44 with 100mm Mineral wool




VISAKA INDUSTRIES LIMITED

Contact Us

( *represents compulsory fields )

Tips on getting accurate quotes. Please include product name, order quantity, usage, special requests if any in your inquiry.



Click here more details...

Part 1

Part 2

Part 3

Part 4

Contact Details
VISAKA INDUSTRIES LIMITED All Rights Reserved.